產(chǎn)品參數(shù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
其它性能 | 射出 | ASTM D-638/D-882 | 220 | % | ||
鑄膜成型 | ASTM D-638/D-882 | 750 | % | |||
薄膜 | MD | ASTM D-638/D-882 | 250 | kg/cm2 | ||
TD | ASTM D-638/D-882 | 240 | kg/cm2 | |||
薄膜 | MD | ASTM D-638/D-882 | 480 | % | ||
TD | ASTM D-638/D-882 | 640 | % | |||
機(jī)械性能 | 沖擊強(qiáng)度 | ASTM D-1709 | 430 | G/F50 | ||
其它性能 | 射出 | ASTM D-638/D-882 | 117 | kg/cm2 | ||
VA含量 | ASTM USIFE | 18 | % | |||
密度 | ASTM D-1505 | 0.939 | g/cm3 | |||
融化點(diǎn) | ASTM D-2117 | 86 | ℃ | |||
VICAT 軟化點(diǎn) | ASTM D-1525 | 64 | ℃ | |||
熔融指數(shù) | ASTM D-1238 | 2.5 | g/10min | |||
低溫易脆性 | ASTM D-746 | <-76 | ℃/F50 | |||
硬度 | ASTM D-2240 | 31 | Shore D | |||
鑄膜成型 | ASTM D-638/D-882 | 180 | kg/cm2 |